MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lotte Chemical Titan TITANLENE® LDF260GG Low density polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: LDF260GG is a low density polyethylene resin for film extrusion. LDF260GG has medium slip and anti-block additives. LDF260GG meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 2.1 & (c) 2.2.

Applications:

  • Laundry film
  • Textile packaging
  • Produce film
  • Diaper backing

Additives:

  • Medium slip
  • Antiblock

Advantages:

  • Good drawdown
  • Excellent process ability

Information provided by Titan Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Base Resin Density 0.922 g/cc0.0333 lb/in³ASTM D1505
Thickness 30.0 microns1.18 milextruded at 2.5:1 BUR
Base Resin Melt Index 5.0 g/10 min5.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 250 %250 %ASTM D882
Film Elongation at Break, TD 440 %440 %ASTM D882
Elmendorf Tear Strength, MD 9.50 g/micron241 g/milASTM D1922
Elmendorf Tear Strength, TD 4.00 g/micron102 g/milASTM D1922
Dart Drop 2.50 g/micron63.5 g/milASTM D1709
Film Tensile Strength at Break, MD 19.6 MPa2840 psiASTM D882
Film Tensile Strength at Break, TD 17.7 MPa2570 psiASTM D882
1% Secant Modulus, MD 186.32 MPa27024 psiASTM D882
1% Secant Modulus, TD 205.94 MPa29869 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 93.0 °C199 °Fresin; ASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 7.0 %7.0 %ASTM D1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 160 - 180 °C320 - 356 °F
Blow-up Ratio (BUR) 2.52.5
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lotte Chemical Titan TITANLENE® LDF260FG Low density polyethylene
Braskem BI 818 LDPE Injection Molding Polyethylene
Chevron Phillips 4538B LDPE Injection Molding Resin
Chevron Phillips KN 230B LDPE Injection Molding Resin
Braskem BC818 Extrusion Coating Low Density Polyethylene

PTITAN69 / 70435

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.