MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Kraton® D4271 J (O/E SBS) Branched Block Copolymer
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: Description: Kraton D4271 J is an oil-extended branched block copolymer based on styrene and butadiene, with bound styrene of 45% mass. It is supplied from Japan in the physical forms identified in the grade nomenclature:
D4271 JSP - supplied as dusted pellets
D4271 JS - supplied as dusted crumb

Region: Japan

Uses: Kraton D4271 J is used for formulating compounds for footwear and general purpose applications and as a modifier of bitumen

Applications: Compounding and Personal Hygiene

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.940 g/cc0.940 g/cc
Volatiles <= 1.0 %
@Temperature 110 °C,
Time 7200 sec
<= 1.0 %
@Temperature 230 °F,
Time 2.00 hour
Melt Flow 6.0 - 14 g/10 min
@Load 5.00 kg,
Temperature 200 °C
6.0 - 14 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Ash <= 1.0 %<= 1.0 %ISO 247
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 72
@Time 30.0 sec
72
@Time 0.00833 hour
ISO 7619
Tensile Strength 16.0 MPa2320 psiISO 37
Elongation at Break 1000 %1000 %ISO 37
300% Modulus 2.00 MPa
@Strain 300 %
290 psi
@Strain 300 %
ISO 37
 
Descriptive Properties
ContentBound Styrene45 percent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kraton® D1155 E (SBS) Liner Block Copolymer
INEOS Styrolution K-Resin® KR03 Styrene Butadiene Copolymer (SBC)
INEOS Styrolution K-Resin® KR01 Styrene Butadiene Copolymer (SBC)
A. Schulman Diamond SBS 1031 Clear Styrene Butadiene Copolymer
Kraton® D1155 B (SBS) Liner Block Copolymer

PKRA9849 / 132748

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.