MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Ovako S355J2 SB9813 Steel, +AR
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: General Information: S355J2 is a structural carbon-manganese steel suitable for e.g. mechanical engineering applications. Below, a number of closely related variants are presented.
520 M is M-steel variant of S355J2 is as rolled or normalize rolled contrition. 550M is drawn or peeled version of S355

Information provided by Ovako

Key Words: ASt 52, A52 FP, Q420q-D, 1501 Gr.224-460, A52 RBII
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell  160 - 180
@Thickness <=16.0 mm
160 - 180
@Thickness <=0.630 in
 160 - 180
@Thickness 16.0 - 40.0 mm
160 - 180
@Thickness 0.630 - 1.57 in
Tensile Strength  520 - 600 MPa
@Thickness <=16.0 mm
75400 - 87000 psi
@Thickness <=0.630 in
 520 - 600 MPa
@Thickness 16.0 - 40.0 mm
75400 - 87000 psi
@Thickness 0.630 - 1.57 in
Tensile Strength, Yield  >= 345 MPa
@Thickness 16.0 - 40.0 mm
>= 50000 psi
@Thickness 0.630 - 1.57 in
Rel
 >= 355 MPa
@Thickness <=16.0 mm
>= 51500 psi
@Thickness <=0.630 in
Rel
Elongation at Break  25 %
@Thickness <=16.0 mm
25 %
@Thickness <=0.630 in
 25 %
@Thickness 16.0 - 40.0 mm
25 %
@Thickness 0.630 - 1.57 in
Modulus of Elasticity 210 GPa30500 ksi
Poissons Ratio 0.300.30
Shear Modulus 80.0 GPa11600 ksi
Impact Test  40.0 J
@Thickness <=16.0 mm,
Temperature -20.0 °C
29.5 ft-lb
@Thickness <=0.630 in,
Temperature -4.00 °F
 40.0 J
@Thickness 16.0 - 40.0 mm,
Temperature -20.0 °C
29.5 ft-lb
@Thickness 0.630 - 1.57 in,
Temperature -4.00 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000200 - 0.00000250 ohm-cm0.00000200 - 0.00000250 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 - 300 °C
6.67 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.460 - 0.480 J/g-°C
@Temperature 50.0 - 100 °C
0.110 - 0.115 BTU/lb-°F
@Temperature 122 - 212 °F
Thermal Conductivity 40.0 - 45.0 W/m-K278 - 312 BTU-in/hr-ft²-°FAmbient temperature
Transformation Temperature 400 °C752 °FMS
 720 °C1330 °FAC1
 815 °C1500 °FAC3
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al >= 0.025 %>= 0.025 %
Carbon, C 0.13 - 0.18 %0.13 - 0.18 %
Chromium, Cr <= 0.15 %<= 0.15 %
Copper, Cu <= 0.30 %<= 0.30 %
Iron, Fe 97.33 - 98.67 %97.33 - 98.67 %As Balance
Manganese, Mn 1.0 - 1.3 %1.0 - 1.3 %
Molybdenum, Mo <= 0.070 %<= 0.070 %
Nickel, Ni <= 0.25 %<= 0.25 %
Phosphorus, P <= 0.025 %<= 0.025 %
Silicon, Si 0.15 - 0.25 %0.15 - 0.25 %
Sulfur, S <= 0.025 %<= 0.025 %
Vanadium, V 0.030 - 0.12 %0.030 - 0.12 %
 
Descriptive Properties
WeldabilityCEV 0.44max
 Pcm 0.25max

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ovako S355J2 S355J2(M) Steel, +AR
Ovako S355JR EN10025-2:2004 Steel
Ovako S355J2 S355K2 Steel, +AR
Ovako S355JR Steel, +AR
Ovako S355J2 EN10025-2:2004 Steel, +AR

NOVAKO412 / 234711

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.