MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Toray TORELINA™ PPS Resin A400M-X05 Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled

Material Notes: GF + mineral filler reinforced, high filler, high strength. Color black. PPS-GF+MD60

General Torelina™ Notes: TORELINA PPS is used to form a complex with an inorganic substance such as glass fiber, and is particularly excellent among thermoplastic resins in terms of its properties such as heat resistance, rigidity, dimensional stability, moist-heat resistance, chemical resistance, and flame retardance. This engineering plastic is widely used in mechanical parts, car parts, electrical and electronic parts.

Information provided by Toray Resin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.82 g/cc0.0658 lb/in³ISO 1183
Water Absorption 0.020 %
@Time 86400 sec
0.020 %
@Time 24.0 hour
In 23°C water; ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/in80x80x3mmt; Toray Method
Linear Mold Shrinkage, Transverse 0.0075 cm/cm0.0075 in/in80x80x3mmt; Toray Method
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 122122ISO 2039-2
Tensile Strength 165 MPa23900 psiISO 527-1,2
Elongation at Break 1.1 %1.1 %ISO 527-1,2
Flexural Strength 250 MPa36300 psiISO 178
Flexural Modulus 18.5 GPa2680 ksiISO 178
Charpy Impact, Notched 2.50 J/cm²11.9 ft-lb/in²V-Notched; ISO 179
Taber Abrasion, mg/1000 Cycles 9.09.0ISO 9352
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmIEC 60093
Dielectric Constant 4.9
@Frequency 1e+6 Hz
4.9
@Frequency 1e+6 Hz
60% RH; IEC 60250
Dielectric Strength 20.0 kV/mm508 kV/inIEC 60243-1
Dissipation Factor 0.0020
@Frequency 1e+6 Hz
0.0020
@Frequency 1e+6 Hz
60% RH; IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 18.0 µm/m-°C10.0 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 30.0 µm/m-°C16.7 µin/in-°FISO 11359-2
Melting Point 278 °C532 °FISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 260 °C500 °FISO 75-1,2
Flammability, UL94 V-0
@Thickness 0.360 mm
V-0
@Thickness 0.0142 in
 
Descriptive Properties
Bar Flow (mm)110Toray Method. 320°C, 98 MPa, 1 mmt

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTORAY9021 / 248711

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.