MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Phillips 66 Compounded Gear Oil ISO Grade 680
Categories: Fluid; Lubricant

Material Notes: Phillips 66® Compounded Gear Oil is a high-quality, compounded lubricant developed for the lubrication of industrial and automotive worm gear drives operating at moderate to high temperatures, and for the lubrication of steam engine cylinders and valves. Compounded Gear Oil is formulated with heavy paraffinic base oils compounded with acid-less tallow (fatty oil). It has high film strength and excellent oiliness characteristics for effective lubrication of worm gears. It emulsifies with water to maintain excellent lubricity in the presence of steam and moisture to protect and lubricate cylinder and valve surfaces in steam engines.

Applications:

  • Industrial worm gear drives made with non-ferrous alloys (bronze-on-steel)
  • Differentials on antique automobiles that require a high-viscosity, compounded gear oil
  • Steam engine cylinders and valves
  • Bearings on steam-heated calender or mixer rolls
  • Screw-down bolts and nuts on aluminum and steel rolling mills
  • Heavily loaded, low-speed bearings subject to moisture contamination
  • Cylinders of gas compressors handling wet natural gas
  • Applications where an SAE 140, SAE 190 or SAE 250, API GL-2 gear oil is specified
Features/Benefits:
  • Excellent lubricity for protection of sliding surfaces against scuffing
  • High film strength
  • Emulsifies with water to resist washing
  • Good oxidation resistance and thermal stability
  • Protects against rust and corrosion
  • Non-corrosive to bronze or brass

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.909 g/cc
Density 7.57 lb/gal
Viscosity Measurement 89Index
Saybolt Viscosity at 100°F 3687 SUS
Saybolt Viscosity at 210°F 181 SUS
Kinematic Viscosity at 40°C (104°F) 680 cSt
Kinematic Viscosity at 100°C (212°F) 37 cSt
ASTM Color 8.0ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.20[mg KOH/g]; ASTM D974
 
Thermal PropertiesOriginal ValueComments
Pour Point -5.00 °C
Flash Point >= 300 °C
 
Descriptive Properties
Copper Corrosion1aASTM D130

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON5085 / 198338

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.