MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Unitika FUN-8000
Categories: Polymer; Thermoplastic; Polyarylate

Material Notes: Characteristics:
  • High impact strength
  • High chemical resistance
  • Transparency as high as polycarbonate

Information provided by Unitika Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/ccASTM D792
Water Absorption 0.15 %
@Thickness 3.17 mm,
Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0080 cm/cm
@Thickness 3.00 mm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 66.0 MPaASTM D638
Elongation at Break 78 %ASTM D638
Flexural Strength 81.0 MPaASTM D790
Flexural Modulus 2100 MPaASTM D790
Izod Impact, Notched 450 J/m
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 123 °CASTM D648
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 87 %
@Thickness 3.00 mm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 260 - 280 °C
Middle Barrel Temperature 270 - 290 °C
Front Barrel Temperature 280 - 300 °C
Nozzle Temperature 280 - 300 °C
Mold Temperature 70.0 - 90.0 °Cactual surface temp
Drying Temperature 120 °C
Dry Time 8.00 - 24.0 hour
Back Pressure 0.490 - 1.47 MPagage pressure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Unitika AXG-1500-300 Conditioned
Unitika L-8005
Unitika L-1003PA
Unitika C300VN
Unitika AXG-1500-300 Dry

PUNITIK888 / 177908

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.