MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Abhar Polymer Compounds APXLP12/APCAT12N Silane Cross-linkable Polyethylene Compound
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: APXLP12 is a XLPE pre-grafted polyethylene which can be processed in combination with its catalyst master batch (APCAT12N) in conventional extruders. Cross linking happen by exposing end products to moisture.

Application: APXLP12 is designed for insulation of low voltage wiring and power cables for the range up to 6kV.

Specification: The catalyst masterbatch APCAT12N in combination with the base PABHAR APXLP12 meets the applicable requirements given below when processed using extrusion practice and testing procedure:

    BS 7870-5
  • IEC 60502-1
Typical values reported above (except MFI) are obtained from samples cured in hot water (7 hours @ 95°C)

Information provided by Abhar Polymer Compounds

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.935 - 0.955 g/cc0.0338 - 0.0345 lb/in³ASTM D 792 / IEC 60811-1-3
Melt Flow 5.5 - 6.5 g/10 min
@Load 5.00 kg,
Temperature 190 °C
5.5 - 6.5 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Storage Temperature <= 35.0 °C<= 95.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 48 - 52
@Time 15.0 sec
48 - 52
@Time 0.00417 hour
ASTM D2240
Tensile Strength 11.25 - 15.0 MPa1632 - 2180 psiafter ageing 10 days at 150°C; IEC 60811-1-2
 >= 15.0 MPa>= 2180 psiIEC 60811-1-1
Elongation at Break 225 - 300 %225 - 300 %after ageing 10 days at 150°C; IEC 60811-1-1
 >= 300 %>= 300 %IEC 60811-1-1
Tensile Set  <= 10 %
@Pressure 0.200 MPa,
Temperature 200 °C
<= 10 %
@Pressure 29.0 psi,
Temperature 392 °F
Permanent elongation after cooling; IEC 60811-2-1
 <= 100 %
@Pressure 0.200 MPa,
Temperature 200 °C
<= 100 %
@Pressure 29.0 psi,
Temperature 392 °F
Elongation under load; IEC 60811-2-1
 
Processing PropertiesMetricEnglishComments
Zone 1 160 - 180 °C320 - 356 °F
Zone 2 200 - 210 °C392 - 410 °F
Zone 3 180 - 220 °C356 - 428 °F
Zone 4 200 - 220 °C392 - 428 °F
Die Temperature 220 - 230 °C428 - 446 °F
Head Temperature 210 - 230 °C410 - 446 °F
Screw Cooling Temperature 70.0 - 80.0 °C158 - 176 °F
Drying Temperature 60.0 °C
@Time 28800 - 43200 sec
140 °F
@Time 8.00 - 12.0 hour
air oven in 4-6cm layers

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PABHAR000 / 249433

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.