MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AISI Type S45500 Stainless Steel, hardened at 540°C (1000°F) for 4 hours, air cooled
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T S40000 Series Stainless Steel

Material Notes: Martensitic, age-hardenable, easily formable (annealed), no corrosion in fresh water, resists staining in normal air atmosphere, good resistance to pitting in 5% salt spray and 5% ferric chloride. For use in service temperatures up to 425°C.

Key Words: UNS S45500, AMS 5578, AMS 5617, AMS 5672, AMS 5860, ASTM A313 (XM-16), ASTM A564 (XM-16), ASTM A705 (XM-16), martensitic, T S45506
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 411
@Thickness 1.30 mm
Converted from Rockwell C hardness. Strip
 434
@Thickness 4.10 mm
Converted from Rockwell C hardness. Strip
 422
@Diameter 102 mm
Converted from Rockwell C hardness. Bar
 422
@Diameter 25.4 mm
Converted from Rockwell C hardness. Bar
Hardness, Knoop 451
@Thickness 1.30 mm
Converted from Rockwell C hardness. Strip
 478
@Thickness 4.10 mm
Converted from Rockwell C hardness. Strip
 464
@Diameter 102 mm
Converted from Rockwell C hardness. Bar
 464
@Diameter 25.4 mm
Converted from Rockwell C hardness. Bar
Hardness, Rockwell C 44
@Thickness 1.30 mm
Strip
 46
@Thickness 4.10 mm
Strip
 45
@Diameter 102 mm
Bar
 45
@Diameter 25.4 mm
Bar
Hardness, Vickers 434
@Thickness 1.30 mm
Converted from Rockwell C hardness. Strip
 459
@Thickness 4.10 mm
Converted from Rockwell C hardness. Strip
 446
@Diameter 102 mm
Converted from Rockwell C hardness. Bar
 446
@Diameter 25.4 mm
Converted from Rockwell C hardness. Bar
Tensile Strength, Ultimate 1515 MPa
@Thickness 1.30 mm
Strip
 1515 MPa
@Thickness 4.10 mm
Strip
 1415 MPa
@Diameter 102 mm
Bar
 1450 MPa
@Diameter 25.4 mm
Bar
Tensile Strength, Yield 1450 MPa
@Strain 0.2 %,
Thickness 4.10 mm
Strip
 1450 MPa
@Strain 0.2 %,
Thickness 1.30 mm
Strip
 1340 MPa
@Strain 0.2 %,
Diameter 25.4 mm
Bar
 1345 MPa
@Strain 0.2 %,
Diameter 102 mm
Bar
Elongation at Break 5.0 %
@Thickness 1.30 mm
in 50 mm. Strip
 6.0 %
@Thickness 4.10 mm
in 50 mm. Strip
 12 %
@Thickness 1.30 mm
in 25 mm. Strip
 14 %
@Thickness 4.10 mm
in 25 mm. Strip
 12 %
@Diameter 102 mm
in 50 mm. Bar
 14 %
@Diameter 25.4 mm
in 50 mm. Bar
Modulus of Elasticity 200 GPaTypical for stainless steel
Notched Tensile Strength 1725 MPa
@Diameter 102 mm
Bar
 2000 MPa
@Diameter 25.4 mm
Bar
Charpy Impact 16.0 J
@Diameter 102 mm
Bar
 27.0 J
@Diameter 25.4 mm
Bar
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000900 ohm-cmannealed, 0.000075 Ohm-cm when annealed and aged at 510°C for 4 hours and air cooled.
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.6 µm/m-°C
@Temperature 22.0 - 95.0 °C
 10.8 µm/m-°C
@Temperature 22.0 - 150 °C
 11.2 µm/m-°C
@Temperature 22.0 - 205 °C
 11.7 µm/m-°C
@Temperature 22.0 - 260 °C
 12.1 µm/m-°C
@Temperature 22.0 - 315 °C
Specific Heat Capacity 0.480 J/g-°CTypical value for stainless steel.
Thermal Conductivity 18.0 W/m-K
@Temperature 100 °C
 19.7 W/m-K
@Temperature 200 °C
 21.3 W/m-K
@Temperature 300 °C
 23.4 W/m-K
@Temperature 400 °C
 24.7 W/m-K
@Temperature 500 °C
Maximum Service Temperature, Air 425 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.050 %
Chromium, Cr 11.8 %
Copper, Cu 2.0 %
Iron, Fe 73 %
Manganese, Mn <= 0.50 %
Molybdenum, Mo <= 0.50 %
Nickel, Ni 8.5 %
Niobium, Nb (Columbium, Cb) 2.0 %
Phosphorus, P <= 0.040 %
Silicon, Si <= 0.50 %
Sulfur, S <= 0.030 %
Titanium, Ti 1.1 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Type S45500 Stainless Steel, annealed at 815°C (1500°F) for 30 minutes, water quenched, bar
Huntsman IROGRAN® PS 455-204 TPU-Polyester
Overview of materials for Air-Hardening Steel
302 Stainless Steel, 60% cold reduction
305 Stainless Steel, annealed, wire

MQM455G / 13840

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.