Availability: Asia Pacific Filler/Reinforcement: Calcium Carbonate, 40% Filler by Weight Features: UV Resistant Uses: Appliance Components; Industrial Applications Form: Pellets Processing Method: Injection Molding Information provided by Teknor Apex |