MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Reynolds Sorta-Clear® 12 Silicone Rubber Compounds
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Product Overview: SORTA-Clear™ Series rubbers are premium water white translucent silicone rubbers (platinum catalyst) which cure at room temperature with negligible shrinkage. Available in Shore 12A, 18A, 37A and 40A hardness, these rubbers feature high tensile and tear strength. SORTA-Clear™ 12 and SORTA-Clear™ 37 offer the convenience of a 1A:1B by volume mix ratio. The 18A and 40A products require a gram scale for measuring parts A + B. SORTA-Clear™ silicones are ideal for making prototype, jewelry or other molds of any configuration where model visibility is important (i.e. extracting a model from the mold via cutting). Materials such as urethane, epoxy or polyester resins can then be cast into SORTA-Clear™ silicone without application of a release agent. Other materials such as wax and low melt metal alloys can also be cast into SORTA-Clear™. SORTA-Clear™ can be pigmented with SILC Pig™ silicone pigments. SORTA-Clear™ 18, SORTA-Clear™ 37 and SORTA-Clear™ 40 are FOOD SAFE and can be used for culinary applications including casting chocolate and other confections. (See separate technical bulletin for usage instructions available at www.smooth-on.com). SORTA-Clear™ 12 is not food safe, and should not be used for food related applications. SORTA-Clear™ 18 is SKIN SAFE and certified by an independent laboratory.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.07 g/cc1.07 g/ccASTM D-1475
Viscosity 6000 cP6000 cPMixed; ASTM D-2393
Linear Mold Shrinkage <= 0.0010 cm/cm<= 0.0010 in/inASTM D-2566
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 1212ASTM D-2240
Tensile Strength 2.21 MPa320 psiASTM D-412
Elongation at Break 590 %590 %ASTM D-412
100% Modulus 0.159 MPa23.0 psiASTM D-412
Tear Strength 14.0 kN/m80.0 pliDie B; ASTM D-624
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 232 °C450 °F
Minimum Service Temperature, Air -53.0 °C-63.4 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 720 min12.0 hour
Pot Life 40.0 min40.0 minASTM D-2471
 
Descriptive Properties
ColorTranslucent
Mix Ratio1A:1Bby volume
 1A:1Bby weight
Specific Volume25.9[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN132 / 296833

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.