MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

ITW Devcon® Tru-Bond™ PSA 2500 Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: The Tru-Bond TM PSA 2500 High Tack Pressure Sensitive Adhesive (PSA) is a one-part, solvent less liquid that cures to a tacky adhesive when exposed to UV/Visible light. This PSA can be cured directly through clear or translucent surfaces or cured first prior to assembly. The curing first method allows for the joining of parts at some future point. This product can bond a wide range of substrates including PE, PP, PET, TPU and most plastics, metals, glass, and ceramics. It can be sprayed, roll coated, bead or brush applied, screen printed or used in a flexographic printing process.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.03 g/cc1.03 g/ccuncured
Volatile Organic Compounds (VOC) Content <= 1.0 g/l<= 1.0 g/lUncured
Water Absorption 1.5 %
@Time 86400 sec
1.5 %
@Time 24.0 hour
cured; ASTM D570
Brookfield Viscosity 2500 cP2500 cPBrookfield RV Spindle 2, 10 rpm
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 93.3 °C200 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Flash Point >= 100 °C>= 212 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Boiling Water (%)1.4Cured. 2 hrs. ASTM D570
ColorClear liquidUncured
 Optically ClearCured
Solubilityketones, oxygenated solventsUncured
ViscosityLow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWD9229 / 239738

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.