MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Dyneon™ PFA 6505TZ Fluoroplastic Granules
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA)

Material Notes: 3M™ Dyneon™ Fluoroplastic Granules PFA 6505TZ (a fully fluorinated copolymer of tetrafluoroethylene and perfluorovinylether) has exceptional temperature resistance, excellent electrical properties and excellent chemical inertness and weather resistance. It is used in molded valves, pumps, tanks, filters, pipes, and in wire and cable applications.

    Features and Benefits:
  • Excellent flexibility
  • Wide service temperature range
  • Excellent, almost universal resistance to solvents and chemicals
  • High transparency
  • Extremely high weathering resistance and UV stability
  • Smooth surfaces
  • Broad processing window
  • High limiting oxygen index: does not support combustion
  • Good non-stick characteristics
  • Excellent electrical insulation properties
  • Excellent mold release
  • Good low friction properties
  • Excellent stress crack resistance

Information provided by the Dyneon division of 3M.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.15 g/ccASTM D792
Melt Flow 5.0 g/10 min
@Load 5.00 kg,
Temperature 372 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60ASTM D2240
Tensile Strength at Break 32.0 MPaASTM D638
Elongation at Break 410 %ASTM D638
Flexural Modulus 550 MPaInjection Molded Bars (0.5"x.125"x 5"); ASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 308 °CASTM D4591
Flammability, UL94 V-0
Oxygen Index >= 95 %ASTM D2863
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent, but thickness not quantified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours Teflon® PFA Grade 450 HP Extrusion and Molding Resin
Chemours Teflon® PFA Grade 950 HP Plus Extrusion and Molding Resin
Daikin NEOFLON® EP-521 Extrusion Grade ETFE
Chemours Tefzel® 750 Fluoropolymer Resin
Chemours Teflon® PFA Grade 440 HP Extrusion and Molding Resin

PDYL9961 / 129979

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.