MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M Dyneon™ THV 340C Fluorothermoplastic  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer

Material Notes: THV 340C is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride in the form of concentrated water-based dispersion containing an ionic emulsifier. It provides a balance of low temperature processing, low flammability, thermal stability, and melt processability. It is designed for coating heat sensitive substrates such as polyester fabrics with its lower fusion temperature and high melt flow index to improve penetration and reflow. It provides a good balance of flexibility, weatherability, chemical resistance, and soil resistance properties in a water-based formulation. No plasticizers are added to achieve flexibility.

Information provided by Dyneon, A 3M Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.95 g/cc1.95 g/ccASTM D792
Solids Content 50 %50 %
Melt Index of Compound 40 g/10 min
@Load 5.00 kg,
Temperature 265 °C
40 g/10 min
@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
 
Thermal PropertiesMetricEnglishComments
Melting Point 145 °C293 °FASTM D4591
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Descriptive Properties
FormConcentrated Water Dispersion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Dyneon™ THV 220G Fluorothermoplastic
3M Dyneon™ THV™ 400 Fluorothermoplastic
3M Dyneon™ THV™ 500 Fluorothermoplastic
3M Dyneon™ THV 220A Fluorothermoplastic
3M Dyneon™ THV 221GZ Fluoroplastic Granules

PDYNE024 / 34832

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.