MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

SABIC NORYL™ Resin 731S Polyphenylene Ether + PS (PPE+PS) (Asia)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ 731S resin is a non-reinforced blend of Polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable resin is FC EU, FDA food contact compliant and has NSF/ANSI 61, ACS, WRAS, and KTW/W270 listings for selected colors and manufacturing locations. NORYL 731S resin exhibits good surface appearance, high ductility, low moisture absorption, dimensional and hydrolytic stability. NORYL 731S resin is an excellent candidate for a variety of water management applications such as valves, filtration components, and water meter internals.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/ccASTM D792
Water Absorption 0.060 %
@Time 86400 sec
0.060 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 58.0 MPa8410 psi50 mm/min; ASTM D638
Elongation at Break 30 %30 %50 mm/min; ASTM D638
Flexural Strength 93.0 MPa13500 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.42 GPa351 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 208 J153 ft-lbASTM D256
 133 J
@Temperature -40.0 °C
98.1 ft-lb
@Temperature -40.0 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.65
@Frequency 50.0 - 60.0 Hz
2.65
@Frequency 50.0 - 60.0 Hz
ASTM D150
Arc Resistance 60 - 120 sec60 - 120 secASTM D495
Comparative Tracking Index 250 - 400 V250 - 400 VUL 746A
Hot Wire Ignition, HWI 60 - 120 sec
@Thickness >=1.50 mm
60 - 120 sec
@Thickness >=0.0591 in
UL 746A
High Amp Arc Ignition, HAI  15 - 30 arcs
@Thickness >=3.00 mm
15 - 30 arcs
@Thickness >=0.118 in
UL 746A
 30 - 60 arcs
@Thickness >=1.50 mm
30 - 60 arcs
@Thickness >=0.0591 in
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/min>= 5.91 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 130 µm/m-°C
@Temperature -40.0 - 60.0 °C
72.2 µin/in-°F
@Temperature -40.0 - 140 °F
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi)  117 °C
@Thickness 3.20 mm
243 °F
@Thickness 0.126 in
unannealed; ASTM D648
 126 °C
@Thickness 6.40 mm
259 °F
@Thickness 0.252 in
unannealed; ASTM D648
UL RTI, Electrical 105 °C221 °FUL 746B
UL RTI, Mechanical with Impact 90.0 °C194 °FUL 746B
UL RTI, Mechanical without Impact 105 °C221 °FUL 746B
Flammability, UL94 HB
@Thickness >=1.50 mm
HB
@Thickness >=0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 310 °C536 - 590 °FInjection Molding
Mold Temperature 70.0 - 95.0 °C158 - 203 °F
Drying Temperature 105 - 110 °C221 - 230 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82253 / 290200

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.