Overview- Consistent processability
- High clarity and gloss
- Complies with U.S. FDA 21 CFR 177.1520 (c)3.1a
DOW DS6D21 Polypropylene Resin is intended for use in case film processes. It is particularly suited for applications requiring high clarity. Former Dow grade acquired by Braskem. |