MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Mocom (ALBIS) Vorprodukt® AL PA66 910/2.1 GF8 TCE8 Polyamide 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 10% Glass Fiber Filled

Material Notes: Filler/additive System: special filler, 8% glass fibers. Features: thermal conductive, electrically conductive, heat ageing stabilization. Applications: automotive, machinery, electrical and electronic, lighting, electrical components, radiator systems, cooling system, housings, functional components

Information provided by ALBIS.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.51 g/ccISO 1183
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm
@Time 86400 sec
ISO 294-4
Spiral Flow 25.0 cm
@Thickness 2.00 mm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 52.0 MPaISO 527-1/-2
Elongation at Break 0.70 %ISO 527-1/-2
Tensile Modulus 10400 MPaISO 527-1/-2
Flexural Strength 88.0 MPaISO 178
Flexural Modulus 11700 MPaISO 178
Charpy Impact Unnotched 6.00 kJ/m²ISO 179/1eU
Charpy Impact, Notched 2.00 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Surface Resistance <= 150 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.40 J/g-°C
Thermal Conductivity 3.50 W/m-KThrough Plane; ASTM E 1461
 8.00 W/m-KIntegral; ISO 22007-2
 15.5 W/m-KIn Plane; ASTM E 1461
Melting Point 262 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 245 °CISO 75-1/-2
Vicat Softening Point 246 °CB50; ISO 306
Flammability, UL94 V-0
@Thickness 3.00 mm
Glow Wire Flammability Index 960 °C
@Thickness 1.00 mm
DIN EN 60695
 
Processing PropertiesOriginal ValueComments
Melt Temperature 300 - 320 °Cinjection molding
Mold Temperature <= 100 °Cinjection molding
Drying Temperature 80.0 °C
@Time 7200 - 43200 sec
in desiccant dryer, depends on moisture content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese CoolPoly® D3612 Thermally Conductive Polyamide (PA66/6)
Celanese Zytel® 70G13HS1L BK031 PA66-GF13
Techmer ES HiFill® PA6/6 GF10 IM L BK 10% Glass Filled
Celanese CoolPoly® E3607 Thermally Conductive Polyamide (PA6)
Overview of materials for Epoxy, Thermally Conductive

PALBIS9924 / 221020

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.