MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
United Cast Bar Unibar 200 Continuously Cast Iron
Categories: Metal; Ferrous Metal; Cast Iron; Gray Cast Iron

Material Notes: Offers exceptional machinability and excellent surface finishes, but limited strength and wear resistance. Noise and vibration damping are excellent in this grade.

Unibar-200 is not suitable for hardening applications.

Information provided by United Cast Bar Ltd.

Key Words: EN-1561-GJL-200 GG20; Meehanite GE200
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.30 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 120 - 200
@Load 3000 kg
10 mm ball
Tensile Strength 115 MPa
@Diameter 150 - 300 mm
 130 MPa
@Diameter 80.0 - 150 mm
 155 MPa
@Diameter 40.0 - 80.0 mm
 180 MPa
@Diameter 20.0 - 40.0 mm
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 2.95 - 3.45 %
Iron, Fe 92.63 - 94.26 %as balance
Manganese, Mn 0.55 - 0.75 %
Phosphorus, P 0.10 - 0.20 %
Silicon, Si 2.1 - 2.9 %
Sulfur, S 0.040 - 0.070 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Gray Cast Iron, ASTM A 48 Class 40
ASTM class 30 Standard gray iron test bars, as cast
ASTM class 20 Standard gray iron test bars, as cast
Overview of materials for Gray Cast Iron
United Cast Bar Unibar 250 Continuously Cast Iron

NUNITED01 / 160448

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.