MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teijin Tenax® A rTPWFCX PEEK-HTA40 Composite
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: Tenax®-A rTPWFCX PEEK-HTA40 are recycled thermoplastic chips that derive from Tenax®-E TPWF PEEK-HTA40 semi-preg [PLS #034]. The polymer matrix of PEEK (polyetheretherketone) offers excellent resistance to chemicals and solvents and the utilization of woven Tenax®-E HTA40 a high tenacity carbon fiber, result in a composite offering a woven reinforcement with lightweight mechanical performance. Chips can be supplied as a bulk “molding compound” or molded into a consolidated laminate form (Tenax®-A rTPWFCLX PEEK-HTA40).

Product Benefits

  • Continuous use at elevated temperature
  • Low flammability, smoke and toxicity
  • Resistant to chemicals and solvents
  • Room temperature storage and shipping
  • Compliant to Health, Safety and Environment requirement
Process Benefits
  • Thermo-formable
  • Short cycle time
  • Over-molding
  • Thermoplastic joining technologies(in laminate form)

Information provided by Teijin Carbon America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.76 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 600 MPa0°, 50 % r.h; ASTM D3039
Tensile Modulus 40.0 GPa0°, 50 % r.h; ASTM D3039
Flexural Strength 800 MPa0°, 50 % r.h; ASTM D790
Flexural Modulus 60.0 GPa0°, 50 % r.h; ASTM D790
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 143 °Conset, 50 % r.h

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEIJIN922 / 277932

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.