MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SACO AEI EXTINITY® 0101-205 Non-Halogen Flame Retardant Compound
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Description: EXTINITY® 0101-205 is a natural, non-halogen flame retardant RoHS polyolefin compound. It is designed for use in a wide variety of jacketing and coating applications. This compound has superior fire performance; including slow flame propagation, self-extinguishing characteristics, and low smoke production. EXTINITY® 0101-205 should be extruded with a screw configuration designed to optimize process conditions and throughput.

Information provided by SACO AEI Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.31 g/cc1.31 g/ccASTM D792
Melt Flow 0.20 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.20 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238 Condition E
Storage Temperature 4.44 - 26.7 °C40.0 - 80.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 67
@Time 10.0 sec
67
@Time 0.00278 hour
ASTM D2240
Tensile Strength at Break 18.6 MPa2700 psiASTM D638
Elongation at Break 600 %600 %ASTM D638
Flexural Modulus, 1% Secant 2760 MPa400000 psiASTM D790
Izod Impact, Notched 3.20 J/cm6.00 ft-lb/inASTM D256
Coefficient of Friction 0.200.20[µk], Kinetic; ASTM D1894
Coefficient of Friction, Static 0.200.20[µs]; ASTM D1894
Taber Abrasion, mg/1000 Cycles 0.100.10H-18; ASTM D3389
 
Thermal PropertiesMetricEnglishComments
Oxygen Index 25 %25 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Zone 1 149 - 160 °C300 - 320 °F
Zone 2 166 - 177 °C330 - 350 °F
Zone 3 177 - 188 °C350 - 370 °F
Zone 4 177 - 188 °C350 - 370 °F
Die Temperature 188 - 199 °C370 - 390 °F
Melt Temperature 182 - 193 °C360 - 380 °F
Head Temperature 171 - 182 °C340 - 360 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSACO023 / 249390

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.