MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
CHT Group QM 1125 25 Shore A Addition Cure Moldmaking Material
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: QM 1125 is a two-component, room temperature, addition cure, silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is a good choice for the molding of furniture, picture frames, architectural materials and duplicating silicone for dental lab use. QM 1125 is exceptionally good where highly detailed parts and mold flexibility are required.

Key Features:

  • Low viscosity
  • Fast demold time
  • Casting resin resistance
  • Excellent flexibility
Main Applications:
  • Molds for architectural replication
  • Molds for polyester, epoxy, and rigid or foam polyurethane resin casting
  • Molds for technical articles and prototypes
  • Molds for furniture and picture frame replication
  • Duplicating silicone for dental lab use

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.23 g/ccUncatalyzed A
 1.23 g/ccUncatalyzed B
Viscosity 3480 cPUncatalyzed B
 3960 cPUncatalyzed A
Linear Mold Shrinkage 0.0010 cm/cmCured, 60 mins at 25°C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 26Cured, 60 mins at 25°C
Tensile Strength 1.98 MPaCured, 60 mins at 25°C
Elongation at Break 230 %Cured, 60 mins at 25°C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 204 °C
Minimum Service Temperature, Air -55.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 25.0 °C
Tack-Free Time <= 15.0 hourCatalyzed
Gel Time 2.00 - 5.00 minCatalyzed
 
Descriptive Properties
ColorBeigeUncatalyzed A
 BlueUncatalyzed B
 Light BlueCatalyzed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Silicone Rubber
Kraton® FG1901 + PA-6 blend (20/80)
Arkema OREVAC® 18370 Maleic Anhydride Modified Polyethylene
Arkema OREVAC® 18345 RNP Pipe Coating Binder Resin
Aremco Corr-Paint™ CP4060-S1 High Temperature Protective Coating, Silicone

PACC2040 / 199428

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.