HOSTACOM HRG1329TC is a 42% glass reinforced PP with excellent stiffness and dimensional stability intended for structural applications. Available in black color. Status: Developmental Availability: North America Application: Automotive Parts; Structural Parts Market: Automotive Processing Method: Injection Molding Attribute: Excellent Stiffness; Good Dimensional Stability Information provided by LyondellBasell. |