MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
BASF Ultramid® T KR 4365 G5 Nylon 6/6T, 25% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Product Description: Ultramid® T KR 4365 G5 is a 25% glass fiber reinforced, flame-retardant, injection molding PA6/6T grade. Good mechanical properties, high tracking resistance, low tendency for deposits on electrical contacts, very resistant to electrolytic corrosion, resistant to solder baths; electroplateable. Flame retardant based on red phosphorus.

Availability: Asia Pacific; Europe; North America

Filler/Reinforcement: Glass Fiber, 25% Filler by Weight

Features: Copolymer; Corrosion Resistant; Flame Retardant; Tracking Resistant

Agency Ratings: EC 1907/2006 (REACH)

RoSH Compliance: RoSH Compliant

Forms: Pellets

Processing Method: Injection Molding

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.38 g/ccISO 1183
Water Absorption 1.3 %Equilibrium, 50% RH; ISO 62
Water Absorption at Saturation 5.5 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Stress 13900 psi
@Temperature 80.0 °C
ISO 527-2
 21800 psi
@Temperature 22.8 °C
ISO 527-2
 27800 psi
@Temperature -40.0 °C
ISO 527-2
Elongation at Break 2.5 %
@Temperature 80.0 °C
ISO 527-2
 2.9 %
@Temperature -40.0 °C
ISO 527-2
 3.0 %
@Temperature 22.8 °C
ISO 527-2
Tensile Modulus 1.20e+6 psiISO 527-1
Charpy Impact Unnotched 36.0 ft-lb/in²
@Temperature 22.8 °C
ISO 179
 38.0 ft-lb/in²
@Temperature -30.0 °C
ISO 179
Charpy Impact, Notched 3.30 ft-lb/in²
@Temperature -30.0 °C
ISO 179
 6.20 ft-lb/in²
@Temperature 22.8 °C
ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Dielectric Constant 4.0
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 14.0 µin/in-°F
CTE, linear, Transverse to Flow 31.0 µin/in-°F
Melting Point 563 °FISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 428 °FUnannealed; ISO 75-2/A
UL RTI, Electrical 284 °F
@Thickness 0.762 mm
UL 746B
 284 °F
@Thickness 1.52 mm
UL 746B
 284 °F
@Thickness 3.05 mm
UL 746B
UL RTI, Mechanical with Impact 212 °F
@Thickness 0.762 mm
UL 746B
 221 °F
@Thickness 1.52 mm
UL 746B
 230 °F
@Thickness 3.05 mm
UL 746B
UL RTI, Mechanical without Impact 248 °F
@Thickness 0.762 mm
UL 746B
 266 °F
@Thickness 1.52 mm
UL 746B
 284 °F
@Thickness 3.05 mm
UL 746B
Flammability, UL94 V-2
@Thickness 0.381 mm
 V-0
@Thickness 0.762 mm
 V-0
@Thickness 3.05 mm
 5VA
@Thickness 1.52 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBASG2034 / 310727

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.