MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
INEOS Styrolution Clearblend 165 MBS
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: CLEARBLEND 165 is an impact modified styrene acrylic copolymer blend with excellent clarity and outstanding toughness.
  • Exceptional toughness
  • Low density
  • Ease of processing
  • Low moisture absorption

Information provided by Styrolution

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM D 792
Water Absorption at Saturation 0.10 %
@Temperature 23.0 °C
ASTM D 570
Linear Mold Shrinkage 0.0020 - 0.0060 in/inASTM D 955
Melt Flow 5.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 70ASTM D 785
Tensile Strength, Yield 3000 psiASTM D 638
Elongation at Break 50 %ASTM D 638
Tensile Modulus 220000 psiASTM D 638
Flexural Strength 5400 psiASTM D 790
Flexural Modulus 225000 psiASTM D 790
Izod Impact, Notched 5.00 ft-lb/inASTM D 256
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 480 °F
Vicat Softening Point 201 °FASTM D 1525
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.57
@Wavelength 589.3 nm
Sodium D Line; ASTM D 542
Haze 2.2 %ASTM D 1003
Transmission, Visible >= 90 %
@Wavelength 550 nm
ASTM D 1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 400 - 460 °F
Mold Temperature 80.0 - 130 °F
Drying Temperature 150 °F
@Time 7200 sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
INEOS Styrolution Zylar® 960 MBS
INEOS Styrolution Clearblend 145 MBS
Plaskolite West Optix® CA-990 Impact Modified Acrylic Resin
Covestro Makrolon® 2458 Polycarbonate, Injection Grade
Denka TP-803 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene

PBASF8030 / 159712

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.