Hostacom PPU X9067HS D62813 is an unfilled PP copolymer, with high melt flow rate, high toughness and increased stiffness. Product is available as a customized color matched, pellet form. This grade is delivered in D62813 color version. This product is also available in other colors, new colors can be developed depending on customer requirements. Applications: Automotive Parts, Interior TrimsInformation provided by LyondellBasell. |