MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Momentive Performance Materials GE Sealants & Adhesives All Purpose Silicone 1
Categories: Polymer; Thermoset; Silicone

Material Notes: All Purpose Silicone 1 sealant is 100% waterproof and ideal for a wide range of projects exposed to harsh weather from the attic to the basement. Permanently flexible, it can stretch and move with expansion and contraction and will never break down due to ultraviolet rays or freezing temperatures. This high-quality sealant is resistant to unsightly stain causing mildew growth. It’s easy to apply and offers excellent adhesion to many common building materials including most wood, metal, vinyl siding, drywall/plaster, glass, and plastic. Backed by a lifetime guarantee.

Features: Resists mold with 7-year mold-free product protection. Same-day rain and water-ready. Full cure in 24 hours. 100% silicone is 100% waterproof and 100% weatherproof. Sun-proof and freeze-proof. Meets ASTM C-920 Class 25 specifications. Permanently flexible. Never cracks, shrinks, breaks down, or washes away; Freeze/thaw stability. Non-paintable. Application: All Purpose Silicone 1 sealant is used in a wide variety of applications including windows, doors, siding, trim, and vents, as well as attic/basement applications.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 g/cc1.02 g/ccCured.
Volatile Organic Compounds (VOC) Content <= 36 g/l<= 36 g/lUncured. Excluding water & exempt compounds; WPSTM C1454
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2525ASTM D2240
Tensile Strength 1.47 MPa213 psiASTM D412
Elongation at Break 328 %328 %ASTM D412
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C400 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min24.0 hourFull Cure
Tack-Free Time 30.0 min0.500 hour50% RH; ASTM C679
Working Life 5.00 - 10.0 min5.00 - 10.0 min
 
Descriptive Properties
AppearancePaste
Carb Chem Curing VOC< 3.0 wt%
ColorAlmondM90075
 BlackGE312A
 BrownGE412A
 ClearGE012A
 Light GrayM90076
 WhiteGE112A
Consistency / Sag< 0.1 inchesASTM D2202
Joint Movement Capability0.25ASTM C719.
OdorAcetic Acid (Vinegar)
Rain Ready12 hours
UV & Weathering ResistanceExcellent30 yr study

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMOMEN9940 / 265751

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.