MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ITW Chockfast® Red Epoxy Grouting Compound
Categories: Polymer; Thermoset; Epoxy

Material Notes: CHOCKFAST Red is a three-component, high strength, 100% solids, epoxy grouting compound used to grout large machinery and to support soleplates in all types of foundations. CHOCKFAST Red has an extremely high compressive strength. This along with negligible shrinkage makes it ideal for installing critically aligned machinery within very close tolerances.

USE & BENEFITS: CHOCKFAST Red has the following advantages when compared to conventional cement-based non-shrink grouts: • Impervious to oil • Cures at least three times as quickly • No mixing ratios to measure • Grouts machinery in final aligned position • High physical strength • High impact strength • Resistance to many more chemicals • Strong bond to metal and concrete • Unaffected by weathering and freeze / thaw cycling • Stated physical properties assured • Superior resistance to fatigue.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.06 g/cc2.06 g/cc
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 13.0 MPa1890 psiASTM D638
Flexural Strength 27.75 MPa4025 psiASTM C580
Flexural Modulus 13.8 GPa2000 ksiASTM C580
Compressive Strength 105.1 MPa15250 psiASTM C579 MOD
Compressive Modulus 13.8 GPa2000 ksiASTM C579 MOD
Izod Impact, Notched 0.203 J/cm0.380 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.2 µm/m-°C
@Temperature 0.000 - 60.0 °C
11.2 µin/in-°F
@Temperature 32.0 - 140 °F
ASTM D696
Shrinkage 0.00 %0.00 %Not measurable; ASTM D2566
 
Processing PropertiesMetricEnglishComments
Cure Time  1080 min
@Temperature 32.0 °C
18.0 hour
@Temperature 89.6 °F
approximate
 1440 min
@Temperature 27.0 °C
24.0 hour
@Temperature 80.6 °F
approximate
 2160 min
@Temperature 21.0 °C
36.0 hour
@Temperature 69.8 °F
approximate
 3240 min
@Temperature 16.0 °C
54.0 hour
@Temperature 60.8 °F
approximate
Pot Life 180 min
@Temperature 21.1 °C
180 min
@Temperature 70.0 °F
Approximate
Shelf Life 24.0 Month24.0 MonthIn dry storage
 
Descriptive Properties
Fire Resistanceself extinguishingASTM D635

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWC9021 / 239531

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.