MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Domo TECHNYL® A 218 V35 PA66, 35% glass fiber, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.

Benefits: The product offers an excellent combination between thermal and mechanical properties.

Available in: Asia Pacific, Europe, Latin America and North America

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications

Applications: It is used in a wide variety of industries.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccISO 1183/A
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 150 MPaISO 527 Type 1A
Tensile Stress at Strain 35.0 MPa
@Strain 1 %,
Temperature 120 °C
 45.0 MPa
@Strain 1 %,
Temperature 80.0 °C
 50.0 MPa
@Strain 1 %,
Temperature 60.0 °C
 55.0 MPa
@Strain 2 %,
Temperature 120 °C
 65.0 MPa
@Strain 1 %,
Temperature 23.0 °C
 70.0 MPa
@Strain 2 %,
Temperature 80.0 °C
 70.0 MPa
@Strain 3 %,
Temperature 120 °C
 80.0 MPa
@Strain 2 %,
Temperature 60.0 °C
 80.0 MPa
@Strain 4 %,
Temperature 120 °C
 85.0 MPa
@Strain 3 %,
Temperature 80.0 °C
 85.0 MPa
@Strain 6.0 %,
Temperature 120 °C
 90.0 MPa
@Strain 1 %,
Temperature 0.000 °C
 90.0 MPa
@Strain 4 %,
Temperature 80.0 °C
 95.0 MPa
@Strain 6.0 %,
Temperature 80.0 °C
 100 MPa
@Strain 3 %,
Temperature 60.0 °C
 100 MPa
@Strain 4 %,
Temperature 60.0 °C
 105 MPa
@Strain 2 %,
Temperature 23.0 °C
 105 MPa
@Strain 6.0 %,
Temperature 60.0 °C
 120 MPa
@Strain 1 %,
Temperature -40.0 °C
 125 MPa
@Strain 3 %,
Temperature 23.0 °C
 160 MPa
@Strain 2 %,
Temperature 0.000 °C
 200 MPa
@Strain 2 %,
Temperature -40.0 °C
Elongation at Break 5.0 %ISO 527 Type 1A
Tensile Modulus 8700 MPaISO 527 Type 1A
Flexural Modulus 6800 MPaISO 178
Izod Impact, Notched (ISO) 18.0 kJ/m²ISO 180/1eA
Charpy Impact Unnotched 100 kJ/m²ISO 179/1eU
Charpy Impact, Notched 18.5 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohmIEC 60093
Dielectric Constant 4.0IEC 60250
Dielectric Strength 29.0 kV/mmIEC 60243
Dissipation Factor 0.11IEC 60250
Comparative Tracking Index 600 VSolution A; IEC 60112
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® A 20 V35 PA66, 35% glass fiber, DRY
BASF Ultramid® A3X2G7 35% Glass Filled PA66 (Dry)
Domo TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY
BASF Ultramid® A3X2G7 BK 23187 35% Glass Filled PA66 FR (Conditioned)
BASF Ultramid® A3X2G7 35% Glass Filled PA66 (Conditioned)

PRHOD646 / 137877

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.