Color concentrate recommended for application in PVC compounds for electrical wires and cables. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. Important considerations: - Heavy metal free
- Formulated with organic and inorganic pigments
- PVC resin based (carrier polymer)
- Supplied in pellet form and packaged in 25kg bags
- Recommended use of 2% to 4%
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
|