MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Syensqo (Solvay Specialty Polymers) Catalyst Masterbatch PS/2LR Polyolefin
Categories: Other Engineering Material; Catalyst/Initiator; Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Catalyst Masterbatch PS/2LR is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or steam at high temperature. Catalyst Masterbatch PS/2LR contains a processing aid and a lower reactive agent which in certain conditions improves processing

Antioxidant; Thermal Aging Resistant

Uses: Piping; Plumbing Parts; Potable Water Applications

Processing: Extrusion; Pipe Extrusion

Availability: Asia Pacific; Europe; North America

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Apparent Bulk Density 0.550 g/cc0.0199 lb/in³ASTM D1895
Melt Flow 0.50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.50 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Processing PropertiesMetricEnglishComments
Zone 1 150 - 200 °C302 - 392 °F
Zone 2 150 - 200 °C302 - 392 °F
Zone 3 150 - 200 °C302 - 392 °F
Zone 4 150 - 200 °C302 - 392 °F
Zone 5 150 - 200 °C302 - 392 °F
Die Temperature 210 °C410 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y6153 / 193074

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.