MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Covestro Desmodur® ME-230 + BaytecT20 + Baytec XL B, 67A Polyurethane, MDI-Ester
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characteristics:
Properties:
  • Good abrasion resistance
  • Excellent hydrolysis resistance
  • Low temperature performance
  • High resilience
  • Good microbial resistance
Comments:
  • Suitable for skate board and roller skate wheels
  • Production of seals, gaskets & hydrocyclones
  • Ideal for snow plow blades

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/ccDesmodur ME-230
Viscosity 8.0 cP8.0 cPBaytec XL B
 80 cP80 cPDesmodur ME-230
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6767ASTM D2240
Tensile Strength at Break 16.3 MPa2360 psiASTM D412
Elongation at Break 590 %590 %ASTM D412
100% Modulus 2.07 MPa
@Strain 100 %
300 psi
@Strain 100 %
ASTM D412
200% Modulus 2.69 MPa
@Strain 200 %
390 psi
@Strain 200 %
ASTM D412
300% Modulus 3.52 MPa
@Strain 300 %
511 psi
@Strain 300 %
ASTM D412
Resilience 6868[%], Bayshore; ASTM D2632
Tear Strength 19.3 kN/m110 pliSplit; ASTM D1938
 52.6 kN/m300 pliDie C; ASTM D624
Compression Set 34 %
@Temperature 70.0 °C,
Time 79200 sec
34 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395-B
 
Processing PropertiesMetricEnglishComments
Processing Temperature 45.0 - 60.0 °C113 - 140 °FBaytec XL B
 65.0 °C149 °FDesmodur ME-230
 70.0 °C158 °FBaytec T20
Mold Temperature 80.0 °C176 °F
Pot Life 6.00 - 7.00 min6.00 - 7.00 min
 
Descriptive Properties
AppearanceliquidDesmodur ME-230
 solidBaytec T20
 solidBaytec XL B
Content0.025Parts by weight of Dabco T-12 per 100 parts of Baytec XL B
 0.5-0.7Parts by weight of Dabco 33LV per 100 parts of Baytec XL B
 100Parts by weight of Desmodur ME-230 prepolymer
 1000 EWNCO, Baytec T20
 22.7-23.3%NCO, Desmodur ME-230
 312.92Parts by weight of Baytec T20
 45 EWNCO, Baytec XL B
 9.68Parts by weight of Baytec XL B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow SZ-1175 Silicone Surfactant
Evonik TEGOSTAB® B 8715 LF2
Covestro Desmodur® MS-090 + Baytec XL B/Baytec XL HQEE, 93A/47D Polyurethane, MDI- Ester
Covestro Desmodur® ME-230 + BaytecT20 + Baytec XL B, 97A/55D Polyurethane, MDI-Ester
Covestro Desmodur® ME-230 + BaytecT20 + Baytec XL B, 85A Polyurethane, MDI-Ester

PCOVEST0482 / 202265

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.