MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Adstif HA 686J Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Sheet/Thermoforming Grade

Material Notes: Adstif is a trade name for select polypropylene resins with high crystallinity used to produce customer applications, such as thermoformed containers, injection molded packaging and consumer goods. Adstif's property and performance characteristics include high crystallinity, broad processing window, high stiffness and good dimensional stability.

Adstif HA686J is a thermoforming grade with improved process ability in stretchability, and end use stiffness, impact strength, HDT and clarity.   Typical customer applications are containers made by solid phase pressure forming (SPPF) / thermoforming or blow molding, such as drinking cups, yogurt cups, noodle cups, margarine tubs, dairy cups, trays and bottles for food, that can be hot fillable or microwavable for reheating of food.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D 792
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 108ASTM D785
Tensile Strength, Yield 37.0 MPaASTM D 638
Elongation at Yield 10 %ASTM D 638
Flexural Modulus 1780 MPaASTM D 790
Izod Impact, Notched 50.0 J/m
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 125 °CASTM D648
 
Descriptive Properties
Processing MethodThermoforming

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ineos H02C-00 Polypropylene Homopolymer
Formosa Plastics Formolene® 5142K Extrusion - Sheet - Thermoforming Polypropylene
Formosa Plastics Formolene® 4142K Extrusion - Sheet - Thermoforming Polypropylene
Dow 560.01 Performance Polypropylene Polymer
Dow 500.00 Performance Polypropylene Polymer

PEQT7023 / 218662

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.