MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Qualchem Danamid FGF-20 Polyamide 6, 20% Glass Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Reinforced with glass fiber.

Information provided by Qualchem Zrt.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.26 g/cc0.0455 lb/in³DIN 53479
Filler Content 18 - 22 %18 - 22 %
Moisture Absorption at Equilibrium 2.0 - 2.2 %2.0 - 2.2 %DIN 53714
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 110 MPa>= 16000 psi50 mm/min; ISO 527-1,2
Elongation at Break 4.0 %4.0 %ISO 527-1,2
Tensile Modulus 5.70 GPa827 ksiISO 527-1,2
Flexural Strength 200 MPa29000 psi10mm/min; DIN 53452
Charpy Impact Unnotched >= 2.00 J/cm²
@Temperature 23.0 °C
>= 9.52 ft-lb/in²
@Temperature 73.4 °F
DIN 53453
Charpy Impact, Notched >= 0.500 J/cm²
@Temperature 23.0 °C
>= 2.38 ft-lb/in²
@Temperature 73.4 °F
DIN 53453
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmDIN 53482
Comparative Tracking Index 550 V550 VIEC 112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 200 °C392 °FDIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 190 °C374 °FDIN 53461
Flammability, UL94 HB
@Thickness 4.00 mm
HB
@Thickness 0.157 in
MSZ 10383

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PQUALC33 / 58445

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.