Chemical setting. Single-part ceramic for glass-to-metal areas up to 1" diam. x 3/4" deep. Used to pot small temperature sensors, gas igniters, and high intensity lights. Applied in areas up to 1" diameter by 1" depth, then air set for 2-4 hours and cured at 200 ºF prior to operation. Two-part systems are used to produce high temperature molds and fixtures. |
Aremco’s ceramic and graphite adhesives are ideal for bonding, potting and sealing probes, sensors, halogen lamps, igniters, power resistors, cartridge heaters, filters, fiberoptics, honeycombs, and graphite structures to 3200°F (1760°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |