MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Elastosil® R plus 4450/60 Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: ELASTOSIL® R plus 4450/60 is a one-part, addition curing blend for the production of compression molded articles. The vulcanizates are black and are notable for their good mechanical properties as well as for their high heat resistance. ELASTOSIL® R plus 4450/60 has very good resistance to hot air at temperatures of 250°C to 300°C.Curing and postcuring do not produce any cleavage products typically formed when peroxides decompose. The curing rate is much higher than that of peroxide systems. Cure time is reduced to 30 - 50 % depending on the wall thickness.

Special features:

  • good hot air resistance
  • easy demolding
  • dry surface
  • no unpleasant smell caused
Application: The product is suitable for the production of compression molded technical articles requiring high resistance to air hotter than 250 °C.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccISO 1183-1 A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60DIN 53505
 58
@Treatment Temp. 250 °C,
Time 605000 sec
Hot-air resistance; DIN 53505
 61
@Treatment Temp. 250 °C,
Time 1.21e+6 sec
Hot-air resistance; DIN 53505
 62
@Treatment Temp. 300 °C,
Time 259000 sec
Hot-air resistance; DIN 53505
 65
@Treatment Temp. 250 °C,
Time 2.42e+6 sec
Hot-air resistance; DIN 53505
 67
@Treatment Temp. 300 °C,
Time 432000 sec
Hot-air resistance; DIN 53505
 71
@Treatment Temp. 300 °C,
Time 605000 sec
Hot-air resistance; DIN 53505
Tensile Strength at Break 8.50 MPaDIN 53504 S3
 5.40 MPa
@Treatment Temp. 300 °C,
Time 432000 sec
Hot-air resistance; DIN 53504 S3
 5.50 MPa
@Treatment Temp. 300 °C,
Time 605000 sec
Hot-air resistance; DIN 53504 S3
 5.50 MPa
@Treatment Temp. 250 °C,
Time 1.21e+6 sec
Hot-air resistance; DIN 53504 S3
 5.60 MPa
@Treatment Temp. 250 °C,
Time 2.42e+6 sec
Hot-air resistance; DIN 53504 S3
 5.70 MPa
@Treatment Temp. 300 °C,
Time 259000 sec
Hot-air resistance; DIN 53504 S3
 6.10 MPa
@Treatment Temp. 250 °C,
Time 605000 sec
Hot-air resistance; DIN 53504 S3
Elongation at Break 430 %DIN 53504 S3
 170 %
@Treatment Temp. 300 °C,
Time 605000 sec
Hot-air resistance; DIN 53504 S3
 190 %
@Treatment Temp. 300 °C,
Time 432000 sec
Hot-air resistance; DIN 53504 S3
 190 %
@Treatment Temp. 250 °C,
Time 2.42e+6 sec
Hot-air resistance; DIN 53504 S3
 210 %
@Treatment Temp. 300 °C,
Time 259000 sec
Hot-air resistance; DIN 53504 S3
 220 %
@Treatment Temp. 250 °C,
Time 1.21e+6 sec
Hot-air resistance; DIN 53504 S3
 250 %
@Treatment Temp. 250 °C,
Time 605000 sec
Hot-air resistance; DIN 53504 S3
Rebound 60 %DIN 53512
Tear Strength 30.0 kN/mASTM D624 B
Compression Set 15 %
@Temperature 175 °C,
Time 79200 sec
DIN ISO 815-B
 
Processing PropertiesOriginal ValueComments
Cure Time 15.0 min
@Treatment Temp. 165 °C
post cured 4h/200°C
 
Descriptive Properties
Appearanceblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9299 / 204828

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.