DuraGrip® DGR 6040 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6040 NC/BK have
an excellent soft touch feel, will bond to olefinics, and are available in FDA compliant formulations. DuraGrip® is not hygroscopic and under normal conditions does not require drying. Information provided by Advanced Polymer Alloys Former product line of Advanced Polymer Alloys (APA), acquired by A. Schulman in 2014. |