MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polynt POLYCOR® 255X Series Gel Coat
Categories: Polymer; Thermoset

Material Notes: Polynt Composites 255X series gelcoats are formulated specifically for the fiberglass industry where reduced flame propagation properties are needed. Its specific formulation results in a unique hardness that helps to prevent graffiti and scratches. 255X series gelcoats are designed for interior application. Because of the special additives that improve hardness and decrease the flame spread, 255X series are not recommended for parts used under direct sun exposure or prolonged water immersion.

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.27 - 1.32 g/cc0.0459 - 0.0477 lb/in³
Brookfield Viscosity 11000 - 16000 cP11000 - 16000 cPColors, RVF rotor #4 @ 4 rpm
 15000 - 20000 cP15000 - 20000 cPWhites, RVF rotor #4 @ 4 rpm
 
Processing PropertiesMetricEnglishComments
Cure Time 45.0 - 60.0 min0.750 - 1.00 hourTack Free
Gel Time 7.00 - 17.0 min7.00 - 17.0 min1.8% MEKP925
 
Descriptive Properties
Sag ResistanceGood at 20 mils
Thixotropic Index>5.52/20 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYN9264 / 231859

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.