MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Kraiburg TPE THERMOLAST® K TC6MLB Thermoplastic Elastomer, Adhesion to PC, ABS, low hardness  (Unverified Data**)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: The AD1 Series is recommended for applications with excellent adhesion to polar thermoplastics such as ABS, PC and PC/ABS. The compounds are available in natural and black colors.

Typical applications:

  • Ear phones
  • Bumpers
  • Door sills
  • Function and design elements
  • Grommets
  • Handles (hand tools and power tools etc.)
  • Seals
  • Thumb wheels
Material advantages:
  • Easy coloring (compounds in natural colors)
  • Excellent adhesion
  • Excellent processing behavior
  • Insert molding possible
  • Pleasant surface feel (Soft touch)
  • Suitable for automotive-interior
  • UL 94 HB listed
  • UV resistance
Processing Method: Injection Molding

Information provided by Kraiburg TPE. A newer data sheet is available in MatWeb.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³DIN EN ISO 1183-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060DIN ISO 7619
Tensile Strength 4.50 MPa653 psiDIN 53504/ISO 37
Elongation at Break 550 %550 %DIN 53504/ISO 37
Tear Strength 16.5 kN/m94.1 pliDIN ISO 34-1
Peel Strength 6.00 kN/m34.2 pliABS; D41 1916
 6.00 kN/m34.2 pliPC; D41 1916
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 250 °C<= 482 °FCylinder Temperature
Rear Barrel Temperature 180 °C356 °F
Middle Barrel Temperature 210 °C410 °F
Front Barrel Temperature 240 °C464 °F
Mold Temperature 40.0 - 60.0 °C104 - 140 °FA temperature exceeding 80 °C (175 °F) should be avoided
Drying Temperature 60.0 - 80.0 °C
@Time 7200 - 14400 sec
140 - 176 °F
@Time 2.00 - 4.00 hour
Injection Pressure 20.0 - 100 MPa2900 - 14500 psi
Back Pressure 1.97 - 4.90 MPa285 - 710 psi
 
Descriptive Properties
ColorNatural
Hot Runner200-250°CThe runner should be empty after a maximum of 2 - 3 shots.

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Bayblend® T85 XF Polycarbonate + ABS
Covestro Bayblend® KU 2-1514 Polycarbonate + ABS, Flame Retardant Grade
Celanese SO.F.TER Pibiflex® 3567 NAT Copolyester TPE
EMS-Griltech Griltex® D 1365E Copolyester Hotmelt Adhesive (Apparel Interlinings)
Telles Bio-based Natural Plastics™ Aliphatic Copolyester, for Injection Molding

PKRAIA8825 / 171483

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.