Silver End Termination Ink C70709D10 is designed for Barium Titanate Multilayer Ceramics. The ink is designed for application using a Palomar dipping system. It can be used for Chipstar dippers, but the rheology needs of the customer to have to be defined. It has excellent cosmetics and fires to a dense, smooth termination with high bond strength. It is designed to be used with standard Nickel/Tin Plating Systems. The ink has been made at a ready to use viscosity and should be gently stirred before use avoiding introduction of air bubbles. Information provided by Gwent Electronic Materials Ltd. |