MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Techmer ES HiFill® TPU 85A 0152 S1
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Availability: North America

Forms: Pellets

Filler/Reinforcement: Metal

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.52 g/cc0.0549 lb/in³ASTM D792
Water Absorption 0.20 %
@Time 86400 sec
0.20 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8585ASTM D785
Tensile Strength at Break 54.5 MPa7900 psiASTM D638
Elongation at Break 560 %560 %ASTM D638
200% Modulus 7.58 MPa
@Strain 200 %
1100 psi
@Strain 200 %
ASTM D412
Flexural Modulus 0.0862 GPa12.5 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 72.8 °C163 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Laripur® LPR 5260EG Thermoplastic Polyurethane
SK Chemicals SKYTHANE® X590A Polyester Based Thermoplastic Polyurethane Elastomer
SK Chemicals SKYTHANE® U0351C Ink Binder
BASF Elastollan® S90A Polyester Type Polyurethane Elastomer
BASF Elastollan® S 85 A TPUR

PTPC0606 / 136544

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.