MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
SABIC XYLEX™ HX7509HP PC+Polyester (Europe)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/PET Polyester Blend

Material Notes: Medium flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant. EtO and gamma sterilizable.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Density 1.20 g/ccISO 1183
Water Absorption 0.12 %23°C/sat; ISO 62
Moisture Absorption 0.0500 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 11 g/10 min
@Load 2.16 kg,
Temperature 265 °C
cm³/10 min; ISO 1133
 12 g/10 min
@Load 2.16 kg,
Temperature 265 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 62.0 MPa50 mm/min; ISO 527
 63.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 60.0 MPa50 mm/min; ASTM D638
 60.0 MPa50 mm/min; ISO 527
Elongation at Break 133 %50 mm/min; ISO 527
 135 %50 mm/min; ASTM D638
Elongation at Yield 5.8 %50 mm/min; ISO 527
 6.3 %50 mm/min; ASTM D638
Tensile Modulus 2140 MPa50 mm/min; ASTM D638
 2300 MPa1mm/min; ISO 527
Flexural Strength 92.0 MPa2 mm/min; break; ISO 178
Flexural Yield Strength 95.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2250 MPa2 mm/min; ISO 178
 2300 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 854 J/mASTM D256
 70.0 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 9.00 kJ/m²80*10*4; ISO 180/1A
 6.00 kJ/m²
@Temperature -10.0 °C
80*10*4; ISO 180/1A
 8.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 10.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 77.0 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 68.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 104 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 68.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 104 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Thermal Conductivity 0.230 W/m-KISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 119 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 108 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 106 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 125 °CRate B/50; ISO 306
 126 °CRate B/120; ISO 306
 126 °CRate B/50; ASTM D1525
Flammability, UL94 V-2
@Thickness 0.750 mm
UL 94
 
Optical PropertiesOriginal ValueComments
Haze 2.0 %
@Thickness 2.54 mm
ASTM D1003
Transmission, Visible 88 %
@Thickness 2.54 mm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 250 - 270 °CInjection Molding
Zone 1 245 - 260 °C
Zone 2 245 - 270 °C
Zone 3 250 - 270 °C
Melt Temperature 250 - 270 °C
Mold Temperature 45.0 - 60.0 °C
Drying Temperature 65.0 - 80.0 °CInjection Molding
Dry Time 3.00 - 5.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Moisture Content 0.020 %
Back Pressure 0.100 - 0.500 MPa
Shot Size 40 - 80 %
Vent Depth 0.00130 - 0.00200 cm
Screw Speed 20 - 100 rpm
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI11622 / 245089

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.