MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
J6 Polymers JFOAM™ BX-600 Engineered Specialty Foam
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: JFoam™ BX-600-R is the R component of a two component polyurethane system, which when combined with the T component produces a high density polyurethane foam. The foam product satisfies all of the requirements of the fine furniture industry for applications in cabinetry doors, end-pieces, picture frames, plaques, etc. This system has been shown to give improved moisture resistance, low reject rate under humid conditions, high impact strength, fast mold wet-out, better flow, and fast demold.

Information provided by J6 Polymers LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 6.00 lb/ft³cup density, #2 cup
 12.0 lb/ft³molded, overall
Viscosity 200 cPT Component, Polymeric MDI
 2500 cPR Component, Polyol Blend
Storage Temperature 65.0 - 85.0 °F
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 22
@Time 86400 sec
Compressive Strength 340 psi10% deflection, Perpendicular; ASTM D1621
Izod Impact, Unnotched 0.650 ft-lb/inMethod A; ASTM D1761
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
Hand Mix Reactivity106 secSting Time
 48 secCream Time
 94 secTop of Cup Time
Mixing Ratio0.5R Component Water Blown Polyol
 0.5T Component Polymeric MDI
Screw Holding Capability160 lbASTM D1761

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M RPF-C (0.32 g/cc) (Reinforced Polyurethane Foam) Continuous Strand Fiberglass
3M RPF-C (0.24 g/cc) (Reinforced Polyurethane Foam) Continuous Strand Fiberglass
General Plastics LAST-A-FOAM® R-9320 Thermal Isolation Blocks
General Plastics LAST-A-FOAM® TR-20 Polyurethane Foam
ITW Insulation TRYMER® 200L Polyisocyanurate Foam

PJSIX011 / 190938

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.