MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Crosspolimeri FRAGOM PR/720 Flame Retardant Polyolefinic
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: FRAGOM: is the trade-mark of our flame retardant polyolefinic compounds

FRAGOM PR/720: halogen-free flame-retardant polyolefinic thermoplastic compound with high values of temperature index and oxygen index, very easy to process and suitable for cable sheathing.

Certify: CEI2011M1, BS7655LTS1-2-3-4, VDE HM4(K=0,6)

Information provided by Crosspolimeri S.P.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.52 g/cc1.52 g/ccASTM D792
Melt Flow  2.0 g/10 min
@Load 21.6 kg,
Temperature 150 °C
2.0 g/10 min
@Load 47.6 lb,
Temperature 302 °F
IEC 811
 30 g/10 min
@Load 21.6 kg,
Temperature 190 °C
30 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Storage Temperature 12.0 °C53.6 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5252ASTM D2240
Tensile Strength 13.0 MPa1890 psiIEC 811
 14.3 MPa2070 psiHydrocarbons resistance; ENI 018100
 14.3 MPa
@Temperature 110 °C,
Time 605000 sec
2070 psi
@Temperature 230 °F,
Time 168 hour
Heat Ageing; IEC 811
 15.6 MPa
@Temperature 70.0 °C,
Time 14400 sec
2260 psi
@Temperature 158 °F,
Time 4.00 hour
Oil resistance, SAE 20; IEC 811
 15.6 MPa
@Temperature 70.0 °C,
Time 14400 sec
2260 psi
@Temperature 158 °F,
Time 4.00 hour
Oil resistance, ASTM II; IEC 811
Elongation at Break 150 %150 %IEC 811
 165 %165 %Hydrocarbons resistance; ENI 018100
 127.5 %
@Temperature 110 °C,
Time 605000 sec
127.5 %
@Temperature 230 °F,
Time 168 hour
Heat Ageing; IEC 811
 180 %
@Temperature 70.0 °C,
Time 14400 sec
180 %
@Temperature 158 °F,
Time 4.00 hour
Oil resistance, SAE 20; IEC 811
 180 %
@Temperature 70.0 °C,
Time 14400 sec
180 %
@Temperature 158 °F,
Time 4.00 hour
Oil resistance, ASTM II; IEC 811
 
Thermal PropertiesMetricEnglishComments
Hot Ball Pressure Test 90.0 °C
@Time 14400 sec
194 °F
@Time 4.00 hour
35%, Penetration (K=0,6); IEC 811
Oxygen Index 40 %40 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Zone 1 110 °C230 °F
Zone 2 135 °C275 °F
Zone 3 150 °C302 °F
Zone 4 160 °C320 °F
Die Temperature 170 °C338 °F
Head Temperature 165 °C329 °F
Dry Time  2.00 hour
@Temperature 80.0 °C
2.00 hour
@Temperature 176 °F
 3.00 hour
@Temperature 90.0 °C
3.00 hour
@Temperature 194 °F
 
Descriptive Properties
Halogen Content< 0,3%IEC 60754-1
Temperature Index Value300°C21% O2, NES 715

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCROS102 / 294186

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.