MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Synthos G 70 Extruded polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Extrusion Grade

Material Notes: Characteristics: Synthos XPS PRIME G is a thermo insulating material, which has been given a shape of a board in the process of extrusion and direct blowing. The product is manufactured from polystyrene resin, the raw material safe for your human health and approved for use in contact with food. It is foam of specific small and closed cell structure containing air in its internal structure. Product does not contain HBCD (hexabromocyclododecane) as flame retardant. Product does not contain blowing agents like CFCs (chlorfluorcarbons), HCFCs (hydrochlorfluorcarbons) or HFCs (hydrofluorcarbons).

Information provided by Synthos

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.350 - 0.470 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 0.200 MPaperpendicular to faces; EN 1607
Modulus of Elasticity 0.0170 GPaat 50% of the peak stress; EN 826
 0.0420 GPain compression; EN 826
Compressive Strength >= 0.250 MPadN = 40, 50, 60 mm, Compressive creep; EN 1606 + AC
 >= 0.250 MPadN = 80, 100, 120 mm, Compressive creep; EN 1606 + AC
 >= 0.300 MPa2% deformation; EN 826
 >= 0.600 MPa5% deformation; EN 826
 >= 0.700 MPa10% relative deformation; EN 826
 >= 0.750 MPaAverage achieved, at 10% deformation; EN 826
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0260 W/m-K
@Temperature -60.0 °C
dN = 40 mm; EN 14307
 0.0270 W/m-K
@Temperature -60.0 °C
dN = 50-100 mm; EN 14307
 0.0270 W/m-K
@Temperature -40.0 °C
dN = 40 mm; EN 14307
 0.0290 W/m-K
@Temperature -40.0 °C
dN = 50-100 mm; EN 14307
 0.0290 W/m-K
@Temperature -20.0 °C
dN = 40 mm; EN 14307
 0.0310 W/m-K
@Temperature -20.0 °C
dN = 50-100 mm; EN 14307
 0.0310 W/m-K
@Temperature 0.000 °C
dN = 40 mm; EN 14307
 0.0330 W/m-K
@Temperature 0.000 °C
dN = 50-100 mm; EN 14307
 0.0330 W/m-K
@Temperature 10.0 °C
dN = 40 mm; EN 14307
 0.0340 W/m-K
@Temperature 10.0 °C
dN = 50-80 mm; EN 14307
 0.0340 W/m-K
@Temperature 20.0 °C
dN = 40 mm; EN 14307
 0.0350 W/m-K
@Temperature 10.0 °C
dN = 100 mm; EN 14307
 0.0350 W/m-K
@Temperature 20.0 °C
dN = 50-80 mm; EN 14307
 0.0360 W/m-K
@Temperature 40.0 °C
dN = 40 mm; EN 14307
 0.0370 W/m-K
@Temperature 40.0 °C
dN = 50-80 mm; EN 14307
 0.0370 W/m-K
@Temperature 20.0 °C
dN = 100 mm; EN 14307
 0.0380 W/m-K
@Temperature 60.0 °C
dN = 40 mm; EN 14307
 0.0390 W/m-K
@Temperature 40.0 °C
dN = 100 mm; EN 14307
 0.0390 W/m-K
@Temperature 60.0 °C
dN = 50-80 mm; EN 14307
 0.0400 W/m-K
@Temperature 70.0 °C
dN = 40-80 mm; EN 14307
 0.0420 W/m-K
@Temperature 60.0 °C
dN = 100 mm; EN 14307
 0.0450 W/m-K
@Temperature 70.0 °C
dN = 100 mm; EN 14307
 
Descriptive Properties
Point load level>5000 NEN 12430, for 5 mm deformation

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSYNTHOS095 / 320376

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.