MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Danquinsa DANCOLL® 245-62AN Primer
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: DANCOLL® 245-62AN is a 20% primer based on a polyether polyurethane. This primer is available in organic solvents. DANCOLL® 245-62AN is used as primer resp. for the impregnation and undercoating onto different textiles, especially onto polyester and polyamide fabrics. DANCOLL® 245-62AN distinguish itself through its extremely good resistance against hydrolyses, microbes and washes. The produced coating based on DANCOLL® 245-62AN is possessing very good adhesive characteristics at the later coating of polyether TPU’s.

Application: DANCOLL® 245-62AN is used for the impregnations of textiles, anchor coats or for the lamination of one and two component applications. For the two component application we would recommend the addition of the isocyanate crosslinker DANCURE 246-06. At the one component application the pre-impregnated textiles can be stored temporarily 6 months until they can be coated with thermoplastic polyurethanes. DANCOLL® 245-62AN can be even used for classic fabric coatings for textile belts, fire hoses and technical textiles. By means of DANCOLL® 245-62AN it can be achieved non-aligned films after the drying process and release of the solvents. Due to its chemical base the films are very good resistant against hydrolysis and microbes.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.990 g/cc0.0358 lb/in³DIN 51.757
Solids Content 19 - 21 %19 - 21 %DIN 53.189
Viscosity 4500 - 8500 cP4500 - 8500 cP
 
Thermal PropertiesMetricEnglishComments
Flash Point 40.0 °C104 °FDIN 51.755
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
AspectTransparent until light yellowish liquid
SolventCyclohexanoneCAS-Nr.: 108-94-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDANQ025 / 294445

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.