MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lord Adhesives Flocklok® 853A Flock Adhesive
Categories: Polymer; Adhesive

Material Notes: LORD Flocklok® 853A is a blocked, heat-curing, singlecoat adhesive used to adhere polyester or nylon flock fibers to a variety of elastomers including EPDM, NR, CR and SBR. Flocked substrates provide good resistance to abrasion.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.9706 - 0.9945 g/cc
Solids Content 46.5 - 50.5 %
Brookfield Viscosity 80 - 200 cPLVT, Spindle #3 @ 30rpm
Viscosity Measurement 35 - 60
@Temperature 25.0 °C
Seconds; Zahn Cup #2
 
Thermal PropertiesOriginal ValueComments
Flash Point 20.0 °CSeta
 
Processing PropertiesOriginal ValueComments
Cure Time 2.50 min
@Temperature 246 °C
 3.00 min
@Temperature 204 °C
Shelf Life 6.00 Month
@Temperature 21.0 - 27.0 °C
 
Descriptive Properties
AppearanceBrown Liquid
SolventsToluene, Xylene, MIBK, Acetates, Aromatic Petroleum Distillates, Acetone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLORD006 / 86014

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.