ME466WG is a 40% mineral-filled polypropylene compound intended for injection molding. This material has a well-balanced ratio of mechanical properties. The product is available in white color. Typical characteristics: - Detergent resistant
- Excellent dimensional stability
- Long term high heat stabilized UL94 Listed
Applications: - Small appliances
- Washing machines, dishwashers and dryers
- White goods
To avoid residual humidity from transport or storage, the material should be pre-dried for approximately 2h at 80°C.Information provided by Borealis AG |