Enable™ performance PE polymers allows film converters to further enhance their business with more stable operations, improve line output and down gauging — in one single polymer for mono- and coextrusion operations. Enable™ 2305 resins are ethylene 1-hexene copolymers. This polymer offers an outstanding balance between processing and film properties, including tensile, impact and puncture. Easier processing and excellent properties lead to significant high pressure LDPE replacement in many applications, yet with superior draw down and enhanced toughness. Enable™2305 resins are available with and without antiblock. TnPP is not intentionally added to Enable™2305 resins. Availability: North America. Additive: antiblock: no; slip: no; processing aid: yes; thermal stabilizer: yes. Applications: agricultural film, food packaging, multilayer packaging film, shrink film, blown film, form fill and seal packaging, stand up pouches, heavy duty bags, collation shrink, lamination film. Forms: pellets. Information provided by ExxonMobil. |