MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Latrobe Lescalloy® HY-TUF VAC-ARC High Strength Alloy Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel; Carbon Steel; Medium Carbon Steel

Material Notes: LESCALLOY HY-TUF VAC-ARC steel is a high strength low alloy steel. It is typically used in the 220/240 ksi (1517/1655 MPa) tensile strength range. At this strength level, the alloy has good ductility, fracture toughness and impact strength. It is vacuum arc remelted to provide optimum cleanliness and preferred ingot structure for superior mechanical properties. This alloy is most frequently used for aircraft landing gear, flap tracks and other structural applications.

Heat Treatment - 940°C - One hour, air cooled; 871°C - One hour, oil quenched; 288°C - Two hours, air cool.

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.281 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 451" from quench end; Jominy End Quench Hardenability
 471/2" from quenched end; Jominy End Quench Hardenability
 471/8" from quenched end; Jominy End Quench Hardenability
Tensile Strength, Ultimate 220 ksi
Tensile Strength, Yield 1276 MPa
Elongation at Break 5.0 %
Reduction of Area 30 %
Fracture Toughness >= 110 MPa-m½
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.3 µm/m-°C
@Temperature 18.0 - 93.0 °C
Thermal Conductivity 37.49 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.25 %
Chromium, Cr 0.30 %
Iron, Fe 94.4 %
Manganese, Mn 1.35 %
Molybdenum, Mo 0.40 %
Nickel, Ni 1.8 %
Silicon, Si 1.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
300M Ultrahigh Strength Steel
AISI 1541 Steel, Annealed and Cold Drawn Bar (UNS G15410)
Latrobe Lescalloy® 300M - HS VAC-ARC High Strength Alloy Steel
Latrobe Lescalloy® HY-180 VIM-VAR ; .375 - 2 thickness High Strength Alloy Steel
Latrobe Lescalloy® 300M VAC-ARC High Strength Alloy Steel

NTIMK019 / 19367

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.