MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mocom (ALBIS) ALCOM® PC+WAL 750/15.1 UV WT1378-04LB PC+ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: Base Polymer: Polycarbonate + Acrylonitrile Butadiene Styrene Blend

Filler/Additive System: 15% Special filler

Special Features: Highly reflective, opaque

Market Segment: Automotive, Electrical and Electronic, Lighting

Application Area: Lighting, light blocking components

Typical Applications: Light guides, reflectors

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.25 g/ccISO 1183
Linear Mold Shrinkage 0.0035 - 0.0065 cm/cm
@Time 86400 sec
ISO 294-4
Melt Flow 22 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 125 MPaH358/30; ISO 2039-1
Tensile Strength, Yield 50.0 MPaISO 527
Elongation at Break 9.5 %ISO 527
Elongation at Yield 3.3 %ISO 527
Tensile Modulus 2900 MPaISO 527
Flexural Strength 85.0 MPaISO 178
Flexural Modulus 3000 MPaISO 178
Charpy Impact Unnotched 80.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 80.0 kJ/m²
@Temperature -40.0 °C
ISO 179/1eU
Charpy Impact, Notched 5.00 kJ/m²
@Temperature -40.0 °C
ISO 179/1eA
 8.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 105 °CISO 75-1/-2
Vicat Softening Point 120 °CB50; ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 93 %Y10 of Reflection; DIN 5033
 0.40 %
@Thickness 0.500 mm
Y10 of Transm.; ISO 13468
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 - 280 °CInjection molding
Mold Temperature 70.0 - 100 °CInjection molding
Drying Temperature 100 - 110 °C
@Time 7200 - 14400 sec
in a dry air (desiccant) dryer
 100 - 110 °C
@Time 14400 - 28800 sec
in air circulating dryer
 
Descriptive Properties
Base PolymerPolycarbonate + Acrylonitrile Butadiene Styrene Blend

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Bayblend® FR 90 Polycarbonate/ABS Blend
Covestro Bayblend® FR 90 N Polycarbonate/ABS Blend
Covestro Bayblend® FR 86 Polycarbonate/ABS Blend
Mocom (ALBIS) ALTECH® PC+ABS ECO 1000/500 PC+ABS
Applied Nanostructured Solutions PC/ABS - Carbon NanoStructure Chopped Fiber Composite

PALBIS8182 / 242241

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.