MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Magnesium
Magnesium Elektron - Service & Innovation in Magnesium

Magnesium Elektron Elektron® Zirmax Hardener Magnesium Alloy
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: Zirmax is a zirconium grain-refiner for magnesium-zirconium alloys containing nominally 33% zirconium micro-particles in a magnesium matrix. Zirmax is specially prepared to enable simple and effective grain refinement of the alloy by the foundry. Good grain refinement is essential in the production of high quality castings.

Applications: Zirmax is a high performance grain refiner for use with Elektron Magnesium-Rare earth alloys such as Elektron® 21, ZE41A, EZ33A, WE43B or QE22A. Zirmax master alloy creates a super-fine equiaxial grain structure in the alloy which promotes high mechanical properties, improved castability and excellent casting integrity.

Magnesium Elektron specification MSS-HD1/00

Information provided by Magnesium Elektron.

Vendors: Magnesium Elektron is the world leader in high strength magnesium alloys in rolled, extruded and cast forms. Phone (303) 589-3189 or visit www.magnesium-elektron.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.30 - 2.40 g/cc2.30 - 2.40 g/cc
 
Component Elements PropertiesMetricEnglishComments
Magnesium, Mg 57 - 69 %57 - 69 %As Balance
Other <= 5.0 %<= 5.0 %Salts
Zirconium, Zr 31 - 38 %31 - 38 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Magnesium AZ92A-T7, Cast
Magnesium Elektron Elektron® AZ80A Magnesium Alloy, UNS M11800
Magnesium Elektron Elektron® AZ31B Magnesium Extrusion Alloy, UNS M11311
Magnesium Elektron Elektron® AM60B Magnesium Alloy
Magnesium Elektron Elektron® AM50A Magnesium Alloy

NMAGEL913 / 186928

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.